Blends of poly(lactic acid) (PLA) and poly(hydroxybutyrate-co-valerate) (PHBV) with different compositions (0–100 wt% PLA, 25 wt% steps) were injection molded into plates of 0.5, 1 and 2 mm thicknesses. The goal of the study was the investigation of the effect of composition and injection molding technology on the enzymatic degradation of the blends. Proteinase K was the only enzyme out of the five used which catalyzed the degradation of PLA, while none of them influenced significantly the hydrolysis of PHBV. PLA and PHBV are immiscible, and their blends have a heterogeneous dispersed structure, but the interaction of the two components is not negligible, and thus influences both structure and degradation. The presence of PHBV hindered the enzymatic hydrolysis of PLA; while neat PLA lost 70 % of its weight upon degradation, the weight loss of PLA phase was only 25 wt% in blends with a PHBV content as low as 25 %. Furthermore, significantly faster degradation was observed on the cut surface compared to the outer, injection molded surface of the samples, explained by the skin-core structure of the blends developed during injection molding. The kinetics of degradation was quantitatively analyzed by modelling and the determining factors of degradation were identified with the help of the parameters obtained.

Factors determining the enzymatic degradation of PLA/PHBV blends / Hegyesi, N., Gigante, V., Vardai, R., Sciancalepore, C., Gallichi-Nottiani, D., Milanese, D., Igricz, T., Aliotta, L., Lazzeri, A., Pukanszky, B.. - In: MATERIALS & DESIGN. - ISSN 0264-1275. - 272:(2026). [10.1016/j.matdes.2026.117447]

Factors determining the enzymatic degradation of PLA/PHBV blends

Sciancalepore C.;Gallichi-Nottiani D.;Milanese D.;
2026-01-01

Abstract

Blends of poly(lactic acid) (PLA) and poly(hydroxybutyrate-co-valerate) (PHBV) with different compositions (0–100 wt% PLA, 25 wt% steps) were injection molded into plates of 0.5, 1 and 2 mm thicknesses. The goal of the study was the investigation of the effect of composition and injection molding technology on the enzymatic degradation of the blends. Proteinase K was the only enzyme out of the five used which catalyzed the degradation of PLA, while none of them influenced significantly the hydrolysis of PHBV. PLA and PHBV are immiscible, and their blends have a heterogeneous dispersed structure, but the interaction of the two components is not negligible, and thus influences both structure and degradation. The presence of PHBV hindered the enzymatic hydrolysis of PLA; while neat PLA lost 70 % of its weight upon degradation, the weight loss of PLA phase was only 25 wt% in blends with a PHBV content as low as 25 %. Furthermore, significantly faster degradation was observed on the cut surface compared to the outer, injection molded surface of the samples, explained by the skin-core structure of the blends developed during injection molding. The kinetics of degradation was quantitatively analyzed by modelling and the determining factors of degradation were identified with the help of the parameters obtained.
2026
Factors determining the enzymatic degradation of PLA/PHBV blends / Hegyesi, N., Gigante, V., Vardai, R., Sciancalepore, C., Gallichi-Nottiani, D., Milanese, D., Igricz, T., Aliotta, L., Lazzeri, A., Pukanszky, B.. - In: MATERIALS & DESIGN. - ISSN 0264-1275. - 272:(2026). [10.1016/j.matdes.2026.117447]
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11381/3079494
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact