The present study focuses on double-lap Friction Stir Welded (FSW) joints in 2024T3 and 7075T6 aluminium alloys subjected to several post-welding-heat treatments at warm (typical aging) and high temperature (solution range) followed by room temperature deformation (tensile tests). The effect of post-welding-heat treatments on the microstructure and mechanical properties of double lap FSW joints were investigated. Polarized Optical Microscopy (POM) and Scanning Electron Microscopy (SEM) analysis reveal a progressive change in grain size and morphology in high temperature post-welding-heat treated joints, leading to Abnormal Grain Growth in the stir zone. Stress–strain curves are rather flat for 200 and 300 C post-welded heat treated joints while, for the other set of samples, stress increases with strain to reach maximum stress of 140–160 MPa. Micro-hardness profiles measured on transversal sections of post-welded heat treated joints reveal conditions (temperature and time) of hardness homogeneity at top, bottom and central nugget zone and/or along the whole measured profile. When homogeneity is reached, fracture occurs in the nugget. A relationship between hardness and tensile properties has been applied in the nugget.

Mechanical properties evolution during post-welding heat treatments of double-lap fsw joints / Cerri, Emanuela; P., Leo. - In: MATERIALS & DESIGN. - ISSN 0264-1275. - 32:(2011), pp. 3465-3475.

Mechanical properties evolution during post-welding heat treatments of double-lap fsw joints

CERRI, Emanuela;
2011-01-01

Abstract

The present study focuses on double-lap Friction Stir Welded (FSW) joints in 2024T3 and 7075T6 aluminium alloys subjected to several post-welding-heat treatments at warm (typical aging) and high temperature (solution range) followed by room temperature deformation (tensile tests). The effect of post-welding-heat treatments on the microstructure and mechanical properties of double lap FSW joints were investigated. Polarized Optical Microscopy (POM) and Scanning Electron Microscopy (SEM) analysis reveal a progressive change in grain size and morphology in high temperature post-welding-heat treated joints, leading to Abnormal Grain Growth in the stir zone. Stress–strain curves are rather flat for 200 and 300 C post-welded heat treated joints while, for the other set of samples, stress increases with strain to reach maximum stress of 140–160 MPa. Micro-hardness profiles measured on transversal sections of post-welded heat treated joints reveal conditions (temperature and time) of hardness homogeneity at top, bottom and central nugget zone and/or along the whole measured profile. When homogeneity is reached, fracture occurs in the nugget. A relationship between hardness and tensile properties has been applied in the nugget.
2011
Mechanical properties evolution during post-welding heat treatments of double-lap fsw joints / Cerri, Emanuela; P., Leo. - In: MATERIALS & DESIGN. - ISSN 0264-1275. - 32:(2011), pp. 3465-3475.
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11381/2677534
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 30
  • ???jsp.display-item.citation.isi??? 29
social impact